MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omnova Solutions Sunigum® P7395 Acrylate Terpolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Acrylate terpolymer partitioned with calcium carbonate. White powder; 1.00 mm particle size; medium viscosity.

Intrinsically resistant to degradation by heat or UV radiation and to many chemicals including oil and fuels. Aesthetic qualities include bringing softness, matte surface finish, and leather-like appearance. It was developed for thermoplastic melt processing with a variety of resins such as PVC, CPE, COPE, TPU, ASA/ABS/SAN and other polymers with some polarity such as olefin copolymers EVA, EMA (20% min copolymer). Sumigum's basic properties and flexibilizing potential allow users to tailor-make softer grades of general purpose and engineering grades TPEs where aesthetics, color-retention, and weatherability are of prime importance.

End uses include auto interior skins, auto profiles & moldings, building gaskets, coated fabric and roofing, hose & tubing, skins and leather, wire and cable.

Omnova Solutions acquired this product line with the Eliokem acquisition.

Key Words: Goodyear Chemical; Thermoplastic Elastomer (TPE) modifier
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5353
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -25.0 - -18.0 °C-13.0 - -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Omnova Solutions Sunigum® P95 Acrylate Elastomer
Geon® Performance Solutions 130 Series 136 Polyvinyl Chloride Copolymer (PVC Copolymer)
Engineered Polymer Solutions ABS 550
Formosa Plastics Formolon® 113 PVC
Geon® Performance Solutions 130 Series 137 Polyvinyl Chloride Copolymer (PVC Copolymer)

PGOOD0 / 42269

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.