MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Overview of materials for Gray Cast Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Gray Cast Iron". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 6.80 - 7.34 g/cc0.246 - 0.265 lb/inĀ³Average value: 7.20 g/cc Grade Count:35
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120 - 550120 - 550Average value: 217 Grade Count:38
Hardness, Knoop 173 - 337173 - 337Average value: 249 Grade Count:17
Hardness, Rockwell C 11.4 - 29.011.4 - 29.0Average value: 17.9 Grade Count:14
Hardness, Vickers 161 - 321161 - 321Average value: 235 Grade Count:17
Tensile Strength, Ultimate 115 - 700 MPa16700 - 102000 psiAverage value: 310 MPa Grade Count:38
Tensile Strength, Yield 65.5 - 420 MPa9500 - 60900 psiAverage value: 265 MPa Grade Count:11
Elongation at Break 1.00 - 15.0 %1.00 - 15.0 %Average value: 6.67 % Grade Count:6
Modulus of Elasticity 62.1 - 162 GPa9000 - 23500 ksiAverage value: 118 GPa Grade Count:15
Flexural Yield Strength 421 - 641 MPa61000 - 93000 psiAverage value: 575 MPa Grade Count:5
Compressive Yield Strength 572 - 1380 MPa83000 - 200000 psiAverage value: 943 MPa Grade Count:16
Poissons Ratio 0.240 - 0.3300.240 - 0.330Average value: 0.294 Grade Count:13
Fatigue Strength 68.9 - 207 MPa10000 - 30000 psiAverage value: 119 MPa Grade Count:16
Machinability 0.000 - 125 %0.000 - 125 %Average value: 48.8 % Grade Count:8
Shear Modulus 27.0 - 65.5 GPa3920 - 9500 ksiAverage value: 47.6 GPa Grade Count:13
Shear Strength 149 - 610 MPa21600 - 88500 psiAverage value: 304 MPa Grade Count:15
Izod Impact Unnotched 5.42 - 54.2 J4.00 - 40.0 ft-lbAverage value: 29.7 J Grade Count:6
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.60 - 4.00 %2.60 - 4.00 %Average value: 3.33 % Grade Count:32
Chromium, Cr 0.0500 - 2.50 %0.0500 - 2.50 %Average value: 0.464 % Grade Count:11
Copper, Cu 0.0500 - 7.50 %0.0500 - 7.50 %Average value: 0.887 % Grade Count:10
Iron, Fe 65.1 - 95.3 %65.1 - 95.3 %Average value: 92.8 % Grade Count:32
Magnesium, Mg 0.0400 - 0.0700 %0.0400 - 0.0700 %Average value: 0.0550 % Grade Count:5
Manganese, Mn 0.100 - 1.50 %0.100 - 1.50 %Average value: 0.610 % Grade Count:32
Molybdenum, Mo 0.0500 - 0.600 %0.0500 - 0.600 %Average value: 0.122 % Grade Count:9
Nickel, Ni 0.0500 - 17.5 %0.0500 - 17.5 %Average value: 1.68 % Grade Count:10
Phosphorus, P 0.0150 - 0.200 %0.0150 - 0.200 %Average value: 0.106 % Grade Count:31
Silicon, Si 1.00 - 3.00 %1.00 - 3.00 %Average value: 2.23 % Grade Count:32
Sulfur, S 0.00500 - 0.150 %0.00500 - 0.150 %Average value: 0.0985 % Grade Count:32

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gray Cast Iron, ASTM A 48 Class 40
Overview of materials for Cast Iron
ASTM class 20 Standard gray iron test bars, as cast
ASTM class 30 Standard gray iron test bars, as cast
SAE J431 automotive gray cast iron, SAE grade G1800

M01017 / 81719

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.