MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 2 to 1 by volume.

TIGA 142-EX is a medium viscosity, sag resistant epoxy adhesive recommended for bonding applications where high shock impact resistance and peel resistance is desired. This two to one ratio, fast setting two-part adhesive is easily mixed and cured at room temperature and develops tough, strong bonds to a wide variety of materials including stainless steel, other metals, glass ceramics and plastics. Fully cured TIGA 142-EX bonds offer superior thermal shock resistance, mechanical, electrical and impact resistant properties and low permeability to gases and vapors. The cured material has good dimensional stability and resistance to water, weather, oxygen and ozone, most petroleum products, mild acids and alkalis and many other chemicals.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccOf resin
 1.47 g/cc
@Temperature 23.0 °C
1.47 g/cc
@Temperature 73.4 °F
Hardener
Viscosity Measurement 3000030000Of hardener
 8000080000Of resin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Tensile Strength at Break 51.0 MPa7400 psi
Elongation at Break 3.5 %3.5 %
Tensile Modulus 2.14 GPa310 ksi
Shear Strength 19.3 MPa
@Temperature 23.0 °C
2800 psi
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 17.7 kV/mm450 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 18.0 min
@Temperature 25.0 °C
18.0 min
@Temperature 77.0 °F
 
Descriptive Properties
ColorIvoryResin
 Light tanHardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding
Master Bond EP36 High Temperature Resistant, Toughened Epoxy System
Master Bond EP21TDC Toughened, Shock Resistant Two Component Epoxy System

PRESINT634 / 65518

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.