MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Buckeye Polymers BP HDPE 9610 R RLK High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Product Information: Our HDPE grade of materials are designed to offer excellent physical properties while providing cost savings versus higher cost prime equivalents. Buckeye Polymers HDPE materials are being used in many applications such as dunnage trays, containers, toys and recreational items.

    Product Features:
  • Large volume availability
  • ISO 9001 approved quality and COA's with each shipment
  • Meets or exceeds GMP.PE.008
  • Easily recyclable at point of molding
  • Appearance: Black

    Forms: Pellets

    Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 - 0.955 g/cc0.0343 - 0.0345 lb/in³ASTM D1505
Melt Flow 6.0 - 10 g/10 min6.0 - 10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 20.0 MPa>= 2900 psiASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Flexural Modulus >= 0.800 GPa>= 116 ksiASTM D790
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis BorPure™ MB7541 High Density Polyethylene for Injection Molding
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Braskem HD7255LS-L HDPE Injection Molding Polyethylene
Buckeye Polymers BP HDPE 9501 R BLK High Density Polyethylene
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin

PBUCK018 / 104486

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.