Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring technology of LPKF (LPKF-LDS®). The product enables selective planting and creation of electric/electronic circuits or antennas on 3D injection-molded carriers. Key properties of Grilamid 1SBVX-50H LDS black:- Suited for Laser Direct Structuring (LDS)
- High stiffness and strength combined with high toughness
- Low moisture adsorption
- High dimensional stability
- Easy processing
- Excellent surface finish
- Outstanding chemical resistance
- Paintable
- Polymer primarily based on renewable resources
Applications: Grilamid 1SBVX-30H LDS black is suitable for thin-walled housings/parts with integrated electrical and mechanical functions found mainly in areas such as telecommunication, electro/electronics or automotive.Information provided by EMS Grivory. |