MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Heraeus Clevios™ P Conductive Sulfonate Polymer for Antistatic Coatings
Categories: Polymer

Material Notes: Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Clevios™ P is an antistatic material based on PEDOT:PSS – chemistry for electronics applications. This conductive polymer possesses high transmission in the visible spectrum transparent colorless to light blue coatings, good resistance to hydrolysis, and good thermal stability.

Typical applications include the antistatic coating of PET or Polycarbonate films for antistatic trays and blister tapes, films for dust protection of components in the LCD industry, antistatic coating of glass, high quality antistatic-coated papers, and other ESD and dissipative applications

Application Methods: Dipping, Spraying, Printing (including gravure, slot-die)

Information provided by Heraeus, Conductive Polymers Division.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 1.2 - 1.4 %1.2 - 1.4 %As Supplied
pH 1.5 - 2.51.5 - 2.5As Supplied
Viscosity 60 - 100 cP60 - 100 cPAs Supplied
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 - 0.100 ohm-cm0.0100 - 0.100 ohm-cmApplied Coating; formulated with DMSO or MEG
Surface Resistivity per Square 1e+051e+05Applied Coating
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 85 %
@Thickness 0.000100 mm
>= 85 %
@Thickness 0.00000394 in
Applied Coating
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month
@Temperature 20.0 °C
9.00 Month
@Temperature 68.0 °F
in unopened original container
 
Descriptive Properties
Form SuppliedLiquid
OdorNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Heraeus Clevios™ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ PH Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Jet 700 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ P Jet N V2 Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ S HT Antistatic/Conductive Polymer Coating for Screen Printing

PHERA990 / 149954

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.