MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent particle distribution and to enhance mechanical properties. Good machinability - use diamond tools and high feed/speed for best results.

Information provided by Aerospace Metal Composites Limited (AMC), acquired by Materion in 2012.

Key Words: Metal Matrix Composite - Silicon Carbide Particle Reinforced Aluminium; Al/SiC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.88 g/cc0.104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 210210Converted from Vickers
Hardness, Rockwell A 58.358.3Converted from Vickers
Hardness, Rockwell B 9595Converted from Vickers
Hardness, Vickers 210210Pryamidal Diamond 10 kg load
Tensile Strength, Ultimate 659 MPa95600 psistatistical analysis gives AVG -3STD at 620 MPa
Tensile Strength, Yield 464 MPa
@Strain 0.2 %
67300 psi
@Strain 0.2 %
statistical analysis gives AVG-3STD at 417 MPa
Elongation at Break 4.0 %4.0 %in 50 mm
Tensile Modulus 115 GPa16700 ksi
Poissons Ratio 0.300.30
Fatigue Strength  210 MPa
@# of Cycles 100000
30500 psi
@# of Cycles 100000
R=-1, Kt=1.75
 300 MPa
@# of Cycles 1.00e+7
43500 psi
@# of Cycles 1.00e+7
RB R=-1
 430 MPa
@# of Cycles 100000
62400 psi
@# of Cycles 100000
R=-1, Kt=1
Fracture Toughness 18.0 - 20.0 MPa-m½16.4 - 18.2 ksi-in½
Shear Modulus 44.0 GPa6380 ksiEstimated from similar metals.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000900 ohm-cm0.00000900 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.5 µm/m-°C
@Temperature -100 - 100 °C
8.61 µin/in-°F
@Temperature -148 - 212 °F
Specific Heat Capacity 0.836 J/g-°C0.200 BTU/lb-°F
Thermal Conductivity 150 W/m-K
@Temperature 0.000 - 100 °C
1040 BTU-in/hr-ft²-°F
@Temperature 32.0 - 212 °F
Melting Point 548 - 660 °C1020 - 1220 °F
Solidus 548 °C1020 °F
Liquidus 660 °C1220 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T7 Forged Plate
Ceramic Process Systems AlSiC-9, 63 vol% SiC

NAMC20 / 14952

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.