MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Arcam ASTM F-75 Cobalt Chrome Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy

Material Notes: ASTM F-75 Cobalt Chromium alloys are widely used in orthopedic implants such as cemented total hip or knee arthroplasty as well as in metal-on-metal bearings in total hip arthroplasty. The alloys feature medium strength and stiffness combined with high corrosion resistance and good biocompatibility.

Information provided by Stratasys®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1030 - 1060 MPa150000 - 154000 psiRm
Tensile Strength, Yield 586 - 614 MPa85000 - 89000 psiRp 0.2
Elongation at Break 17 - 23 %17 - 23 %
Reduction of Area 18 - 22 %18 - 22 %
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.010 %<= 0.010 %
Boron, B <= 0.010 %<= 0.010 %
Carbon, C <= 0.020 %<= 0.020 %
Chromium, Cr 27 - 30 %27 - 30 %
Cobalt, Co 61.2 - 67.83 %61.2 - 67.83 %
Iron, Fe 0.17 %0.17 %
Magnesium, Mg <= 1.0 %<= 1.0 %
Molybdenum, Mo 5.0 - 7.0 %5.0 - 7.0 %
Nickel, Ni <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.10 %<= 0.10 %
Sulfur, S <= 0.010 %<= 0.010 %
Titanium, Ti <= 0.010 %<= 0.010 %
Tungsten, W <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kinetics MIM F75 (ASTM F75) HIP
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
ATI Allvac® REX 734™ UNS S31675 Specialty Steel
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked

NSTRAT009 / 78551

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.