MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation according to ISO: PA 6T/66+X According to ASTM: PPA, polyphthalamide. The main distinguishing feature of Grivory HT-PPA, when compared to other polyamides, is its good performance at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. The special property profile of Grivory XE 4216 black 9233 makes it suitable for automotive parts with very high demands on heat stability. Parts of good surface quality are feasible. Grivory XE 4216 black 9233 is applicable for engine compartment and power-train applications such as:
  • Charge air ducts
  • Charge air cooler tanks
  • Air intake silencers
  • Oil sumps
  • Functional parts

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³Dry; ISO 1183
Water Absorption 5.4 %5.4 %Sim. to ISO 62
Moisture Absorption 2.10 %2.10 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 210 MPa30500 psiConditioned; ISO 2039-1
 260 MPa37700 psiDry; ISO 2039-1
Tensile Strength at Break 150 MPa21800 psiConditioned; ISO 527-1/-2
 190 MPa27600 psiDry; ISO 527-1/-2
Elongation at Break 2.7 %2.7 %Dry; ISO 527-1/-2
 2.7 %2.7 %Conditioned; ISO 527-1/-2
Tensile Modulus 9.60 GPa1390 ksiConditioned; ISO 527-1/-2
 11.0 GPa1600 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 4.50 J/cm²
@Temperature -30.0 °C
21.4 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmDry; IEC 60093
 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 45.0 kV/mm1140 kV/inDry; IEC 60243-1
 45.0 kV/mm1140 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 525 V525 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C44.4 µin/in-°FISO 11359-1/-2
Melting Point 300 °C572 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C302 °FLong Term; ISO 2578
 270 °C518 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 155 °C311 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAir intake systems
 Fuel systems
 Hydraulic systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical equipment
 Energy distribution
 Mobile phones and other portable devices
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
ProcessingInjection Molding
Product AttributesBio based Polyamide
 Co Polyamide
 Improved alcohol resistance
 Partially aromatic Polyamide
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30
Celanese Zytel® 74G33J NC010 PA66+PA6-GF33
EMS-Grivory Grivory® HT1V-3 FWA black 9225 PA6T/6I-GF30

PGRH412 / 157121

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.