MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Braskem PB 608 LDPE Injection Molding Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility properties and very good flow ability.

Applications: Covers and parts with large flat area; injection molding.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ASTM D1505
ESCR 100% Igepal® 15 hour
@Thickness 3.00 mm,
Temperature 23.0 °C
15 hour
@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3939ASTM D2240
Tensile Strength at Break 8.00 MPa1160 psiASTM D638
Tensile Strength, Yield 8.00 MPa1160 psiASTM D638
Elongation at Break 390 %390 %ASTM D638
Flexural Modulus, 1% Secant 450 MPa65300 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 79.0 °C174 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 210 °C356 - 410 °FTemperature profile
Mold Temperature 5.00 - 25.0 °C41.0 - 77.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
Overview of materials for Low Density Polyethylene (LDPE), Molded
Braskem F7018 LDPE Injection Molding Polyethylene
Braskem PB 208 LDPE Injection Molding Polyethylene
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade

PBRAS093 / 27827

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.