MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Touchstone CFOAM® 17 Structural Carbon Foam  (discontinued **)
Categories: Carbon; Other Engineering Material; Composite Core Material

Material Notes: CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally insulating or conducting and whose electrical conductivity can be varied over seven orders of magnitude. It can be fabricated in a variety of shapes, sizes, and densities to meet the property requirements of specific applications.

These foams will not off-gas at elevated temperatures and will not support ignition. Unlike most metals and ceramics, CFOAM mechanical properties do not deteriorate with increased temperature if protected from oxidization, making carbon foams an attractive thermal protection material. Carbon foams also are tolerant to impact damage and can be repaired in-place using carbonaceous adhesives. They can be bonded easily to dissimilar materials, such as metals or PMCs, for oxidation or further impact protection, respectively.

Results from ASTM E1354, ASTM E1515, MIL-STD-1623, Coast Guard IMO, and FTP Code Part I and Part III indicate that CFOAM will pass all key fire tests including radiant panel, smoke generation, toxicity, cone calorimeter, fire resistance, and room corner tests.

Information provided by Touchstone Research Laboratory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.272 g/cc0.00984 lb/in³ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2.07 MPa300 psiASTM C297
Tensile Modulus 0.345 GPa50.0 ksiASTM C297
Compressive Strength 6.21 MPa900 psiASTM C365
Compressive Modulus 0.552 GPa80.0 ksiASTM C365
Shear Strength 1.38 MPa200 psiTorsional Shear
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 - 1.00e+7 ohm-cm0.0100 - 1.00e+7 ohm-cmTailorable; ASTM D4496
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.86 µm/m-°C
@Temperature 20.0 °C
2.70 µin/in-°F
@Temperature 68.0 °F
ASTM E228
Thermal Conductivity 0.250 - 25.0 W/m-K1.74 - 174 BTU-in/hr-ft²-°FTailorable; ASTM E1225
Maximum Service Temperature, Air 600.0 °C1112 °F
Maximum Service Temperature, Inert 3000 °C5430 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Touchstone CFOAM® 25 Structural Carbon Foam
Touchstone CFOAM® 20 Structural Carbon Foam
Touchstone CFOAM® 30 Structural Carbon Foam
Destech Open-Celled Glassy Carbon Foam
Cymat A35620SC 020SS Stabilized Aluminum Foam

ETOUCH00 / 6135

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.