MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ATI Wah Chang TI-45 Nb
Categories: Metal; Nonferrous Metal; Titanium Alloy

Material Notes: Applications: Aerospace Rivet Material; High Pressure Oxygenated Gas Vents; Superconducting Wire

Information provided by ATI Wah Chang

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 5.70 g/cc0.206 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 546 MPa79200 psi
Tensile Strength, Yield 480 MPa69600 psi
Elongation at Break 23 %23 %in 1 in gage
Modulus of Elasticity 62.05 GPa9000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.03 µm/m-°C
@Temperature 20.0 °C
5.02 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 10.0 W/m-K69.4 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Niobium, Nb (Columbium, Cb) 45 %45 %
Titanium, Ti 55 %55 %
 
Descriptive Properties
Thermal Diffusivity, ft²/sec46.3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 36 55Ti-45Nb
ATI Wah Chang Tiadyne™ 3510
Goodfellow Titanium 50/Iron 50 Alloy
Nitinol - NiTi Shape Memory Alloy; High-Temperature Phase
Goodfellow Copper 56.4/Titanium 43.6 Alloy

NATIWC16 / 15071

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.