MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akro-Plastic Akromid® T1 GF 40 natural (3463) PPA Conditioned, 40% Glass Filled
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Description: AKROMID S3 GF 40 natural (3463) is a 40% glass fiber reinforced polyphthalamide with high rigidity and strength, as well as high temperature and chemical resistance and light inherent color.

Features:

  • Good Chemical Resistance
  • High Stiffness
  • High Strength
  • High Heat Resistance

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Filler Content 40 %40 %ISO 1172
Moisture Absorption 1.1 %
@Temperature 70.0 °C
1.1 %
@Temperature 158 °F
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psi5 [mm/min]; ISO 527-2
Elongation at Break 2.1 %2.1 %5 [mm/min]; ISO 527-2
Tensile Modulus 15.5 GPa2250 ksi1 [mm/min]; ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 313 °C595 °FDIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA)
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Akro-Plastic Akromid® T1 GF 50 natural (3376) PPA Dry, 50% Glass Filled
Celanese Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
LATI Latilub 57-30GRTS G/20 PPA, 20% Glass Fiber Reinforced

PAKRO367 / 182954

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.