MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® PTFE Grade 30 Aqueous Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon® PTFE 30 fluoropolymer resin is a negatively charged, hydrophobic colloid containing approximately 60% (by total weight) of 0.05 to 0.5 mm polytetrafluoroethylene (PTFE) resin particles suspended in water. A milky white liquid, Teflon® PTFE 30 also contains approximately 6% (by weight of PTFE) of a nonionic wetting agent and stabilizer. Viscosity at room temperature is approximately 20 cP. Nominal pH is 10.

Compared with other grades of PTFE dispersions,Teflon® PTFE 30 is a general-purpose product, often preferred for impregnating woven goods and for some coating processes. It imparts some of the unique properties of PTFE resin to porous structures.

When properly processed, the PTFE resin in Teflon® PTFE 30 exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Teflon® PTFE 30 is used to impregnate packings made from braided fibers for severe chemical and thermal service; to coat glass fabric for industrial conveyor belting, nonadhesive separator sheets for laminating and press blankets, and gaskets; and as surface coatings for other substrates.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Polytetrafluoroethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D4441
Base Resin Density 0.900 g/cc0.0325 lb/in³Weight of PTFE resin solids; ASTM D4441
Solids Content 60 %60 %Percent of PTFE resin solids; ASTM D4441
Particle Size 0.22 µm0.22 µmAverage dispersion particle size
pH 9.59.5ASTM E70
Viscosity 20 cP
@Temperature 25.0 °C
20 cP
@Temperature 77.0 °F
ASTM D2196
 
Thermal PropertiesMetricEnglishComments
Melting Point 327 °C621 °FASTM D1457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade 305A Aqueous Dispersion
Chemours Teflon® PTFE 7A Granular Molding Powder
Afton Plastics 440HP PFA Compression Molded Rod
Chemours Teflon® PTFE Grade 30B Aqueous Dispersion
Afton Plastics 450HP PFA Welding Rod

PDU9201 / 33320

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.