MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lushan M-12A Adhesive Resin for Multi-layer Oxygen Barrier Pipe
Categories: Polymer; Adhesive; Thermoplastic; Polyolefin

Material Notes: Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethylene vinyl alcohol (EVOH) etc.

Adhesive resin Lushan M-20A & 12A have good properties:

  • High bonding strength
  • A wide range of bonding
  • Excellent chemical bonding with barrier materials EVOH & Nylon
  • Excellent heat resistance, weather resistance, chemical resistance
  • Excellent mechanical properties
  • Easy processing for adhesive resin
  • Hygiene and safety, non-toxic residue for adhesive resin, etc.
Applications: EVOH

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ASTM D1505
Melt Index of Compound 2.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.55 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psiASTM D638
Elongation at Break 720 %720 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 100.6 °C213.1 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.060 %0.060 %HG/T2751
 
Descriptive Properties
AppearanceTransparent particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyram Bondyram® TL1207 Maleic Anhydride Modified Co-Polymer Polypropylene
Polyram Bondyram® 5108 Maleic Anhydride Modified High Density Polyethylene
Polyram Bondyram® 5101 Maleic Anhydride Modified High Density Polyethylene
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe

PLUSH021 / 150019

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.