MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dow LDPE 4005M Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Data provided by Dow Chemical.

Key Words: Dow PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.916 g/cc0.0331 lb/in³
Melt Flow 5.5 g/10 min
@Load 2.16 kg
5.5 g/10 min
@Load 4.76 lb
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 10.3 MPa1490 psi
Tensile Strength, Yield 9.00 MPa1310 psi
Elongation at Break 600 %600 %
Modulus of Elasticity 0.172 GPa24.9 ksiMolded Sample 2% Secant Modulus
Izod Impact, Notched (ISO) 48.0 kJ/m²
@Temperature -50.0 °C
22.8 ft-lb/in²
@Temperature -58.0 °F
Tensile Impact Strength 275 kJ/m²131 ft-lb/in²
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 90.0 °C194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow LDPE 4005 Low Density Polyethylene, Extrusion Coating Grade
Dow LDPE 4012M Low Density Polyethylene
Dow LDPE 5004IM Low Density Polyethylene
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade
Dow LDPE 640IM Low Density Polyethylene

PDW489 / 34558

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.