MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Axiall 5006 Rigid PVC, Extrusion, Natural  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf 5006 is widely used for high gloss custom profile, sheet applications. USDA approval allows for use in walk-in coolers and refrigerated trucks. Single or twin screw machines may be used to convert Georgia Gulf 5006. It has been designed with good impact at ambient temperatures. The high flexural and tensile strength make it highly suitable for structural installation. The extrusion flow characteristics are excellent in complicated profiles. It is easily colored using concentrates.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ASTM D-785
Hardness, Shore D 8282ASTM D-2240
Tensile Strength, Yield 49.0 MPa7100 psiASTM D-638
Tensile Modulus 3.10 GPa450 ksiASTM D-638
Flexural Strength 84.1 MPa12200 psiASTM D-790
Flexural Modulus 3.45 GPa500 ksiASTM D-790
Izod Impact, Notched  0.801 J/cm
@Thickness 6.35 mm
1.50 ft-lb/in
@Thickness 0.250 in
ASTM D-256
 1.33 J/cm
@Thickness 3.17 mm
2.50 ft-lb/in
@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 137 kJ/m²65.0 ft-lb/in²ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.8 µm/m-°C
@Temperature 20.0 °C
36.0 µin/in-°F
@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C156 °FASTM D-648
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 °C365 °F
 
Compliance PropertiesMetricEnglishComments
USDA YesYes
 
Descriptive Properties
Cell Classification13464ASTM D-1784

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall Tuf-Stif 2802 Rigid PVC, Extrusion
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
Axiall 2512 Rigid PVC, Extrusion
Colorite Polymers 9077 Non-Phthalate 77 Series Vinyl Compound
Colorite Polymers 8533 General Purpose Vinyl Compound

PGGUL394 / 41670

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.