MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kolon KOPEL® KP3363 General Purpose TPE Resin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very similar to rubber, but its processability is much superior to rubber. While its flexibility and elastic recovery are similar to rubber, its mechanical properties-heat resistance, weather resistance and UV stability-are far greater than the performance of rubber.

Excellent flexibility and creep resistance, good mechanical properties and heat stability, good chemical resistance

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³DIN 53479; ASTM D792
Water Absorption 0.30 %0.30 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.013 - 0.015 cm/cm0.013 - 0.015 in/inASTM D955
Melt Flow 20 g/10 min
@Temperature 230 °C
20 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565DIN 53505; ASTM D2240
Tensile Strength, Ultimate 37.3 MPa5400 psiDIN 53455; ASTM D638
Elongation at Break 550 %550 %DIN 53455; ASTM D638
Flexural Yield Strength 294 MPa42700 psiDIN 53455; ASTM D790
Resilience 4343
Izod Impact, Notched 0.824 J/cm1.54 ft-lb/inLow Temp
 NBNBDIN 53453; ASTM D256
Taber Abrasion, mg/1000 Cycles 7.07.0CS-17 WHEEL; ASTM D1044
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °FDIN 53461; ASTM D648
Brittleness Temperature <= -70.0 °C<= -94.0 °FSolenoid Brittle Point; ASTM D746
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOPEL® KP3372 General Purpose TPE Resin
EMS-Grivory Grilon® TSZ 1 PA666
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin
Aearo E-A-R Specialty Composites VersaDamp™ V-2775 TPE
Aearo E-A-R Specialty Composites VersaDamp™ V-2750 TPE

PKOL075 / 48981

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.