MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Nylatron® MC® 907 PA6 Natural and Black, Unfilled Type 6 nylon (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
 1.15 g/cc1.15 g/ccASTM D792
Water Absorption 0.60 %0.60 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 7.0 %7.0 %Immersion; ASTM D570(2)
 7.00 %7.00 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
 88.088.0ASTM D785
Hardness, Rockwell R 115115ASTM D785
Hardness, Shore D 80.080.0ISO 868
 8585ASTM D2240
Tensile Strength 82.7 MPa12000 psiASTM D638
 88.0 MPa12800 psiISO 527-1/-2 (7)
Tensile Strength at 65°C (150°F) 41.4 MPa6000 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Elongation at Yield 5.00 %5.00 %ISO 527-1/-2 (7)
Tensile Modulus 2.76 GPa400 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
 121 MPa17500 psiISO 178 (12)
Flexural Modulus 3.45 GPa500 ksiASTM D790
Compressive Yield Strength  34.0 MPa
@Strain 1.00 %
4930 psi
@Strain 1.00 %
ISO 604 (10)
 64.0 MPa
@Strain 2.00 %
9280 psi
@Strain 2.00 %
ISO 604 (10)
 93.0 MPa
@Strain 5.00 %
13500 psi
@Strain 5.00 %
ISO 604 (10)
Compressive Strength 103 MPa15000 psi10% Def.; ASTM D695
Compressive Modulus 2.76 GPa400 ksiASTM D695
Shear Strength 75.8 MPa11000 psiASTM D732
 76.0 MPa11000 psiASTM D732
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256 Type A
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.200.20Dry vs. Steel; QTM55007
K (wear) Factor 201 x 10-8 mm³/N-M100 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.105 MPa-m/sec3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmEOS/ESD S11.11
 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
 3.70
@Frequency 1.00e+6 Hz
3.70
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inShort Term; ASTM D149
 19.7 kV/mm500 kV/inASTM D149
 25.0 kV/mm635 kV/inIEC 60243-1 (15)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM E-831 (TMA)
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
50.0 µin/in-°F
@Temperature 73.4 - 212 °F
 90.0 µm/m-°C
@Temperature -40.0 - 149 °C
50.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.245 W/m-K1.70 BTU-in/hr-ft²-°FASTM F433
 0.245 W/m-K1.70 BTU-in/hr-ft²-°F
 0.290 W/m-K2.01 BTU-in/hr-ft²-°F
Melting Point 216 °C420 °FCrystalline, Peak; ASTM D3418
 216 °C420 °FASTM D3418
Maximum Service Temperature, Air 93.3 °C200 °FLong Term
 93.3 °C200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648
 93.3 °C200 °FASTM D648
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYesNatural Only
Canada AG NoNo
FDA YesYesNatural Only
NSF NoNo
USDA YesYesNatural Only
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
 UnacceptableUnacceptable
Acids, Weak LimitedLimited
 LimitedLimited
Alcohols LimitedLimited
 LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
 UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
 LimitedLimited
Chlorinated Solvents LimitedLimited
 LimitedLimited
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
 LimitedLimited
Hot Water / Steam LimitedLimited
 LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
 AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
 AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
 AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 AcceptableAcceptable
 
Descriptive Properties
ColorNatural
ESd categoryInsulative
Machinability11-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron® MC 901 H. S. Type 6 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® 101 PA66 Extruded, Unfilled, Type 66 Natural and Black (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet)

P1SM21B / 20106

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.