MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B27 SD 05 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: Ultramid® B27 SD 05 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 - 0.740 g/cc0.0231 - 0.0267 lb/in³
Density 1.12 - 1.15 g/cc0.0405 - 0.0415 lb/in³ISO 1183
Viscosity Measurement 2.67 - 2.732.67 - 2.73(RV) 1% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 146 - 151146 - 151(RV) 0.5% [m/v] in 96% [m/m] sulfuric acid; ISO 307
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Decomposition Temperature >= 300 °C>= 572 °F
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.060 %<= 0.060 %ISO 15512
 
Descriptive Properties
Amino end-groups35-39 meq/kgBASF
Commercial StatusEurope
Extractables<0.6 %ISO 6427
Titanium Dioxide Pigment Content0.28 - 0.32ISO 3451-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B27 SD 02 PA6
BASF Ultramid® B27 E PA6
BASF Ultramid® B27 E 01 PA6 (Dry)
BASF Ultramid® B27 E 01 PA6 (Conditioned)
BASF Ultramid® B27 03 PA6

PBASG0376 / 132009

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.