Sumitomo Bakelite E 264H Epoxy Molding Compound
Categories:
Polymer
;
Thermoset
;
Epoxy
;
Epoxy Molding Compound
Material Notes:
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.
Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.82
g/cc
1.82
g/cc
ASTM D792
Water Absorption
0.15 %
@Time 173000 sec
0.15 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage
0.000090
cm/cm
0.000090
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
105
105
ASTM D695
Tensile Strength
94.0
MPa
13600
psi
ASTM D638
Flexural Strength
235
MPa
34100
psi
ASTM D790
Flexural Modulus
20.0
GPa
2900
ksi
ASTM D790
Compressive Strength
203
MPa
29400
psi
ASTM D695
Izod Impact, Notched
7.28
J/cm
13.6
ft-lb/in
ASTM D256A
Electrical Properties
Metric
English
Comments
Dielectric Constant
3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength
>=
15.0
kV/mm
@Frequency 60 Hz
>=
381
kV/in
@Frequency 60 Hz
SS, dry
>=
17.5
kV/mm
@Frequency 60 Hz
>=
445
kV/in
@Frequency 60 Hz
ST, dry
Dissipation Factor
0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance
125
sec
125
sec
ASTM D495
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
282
°C
>=
540
°F
Post Baked; ASTM D648A
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Cosmic Plastics CP7311 Epoxy Molding Compound
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade
Sumitomo Bakelite 52-01 Diallyl Ortho-Phthalate Molding Compound
PSUMIT126 / 193931
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.