MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik ACRYMID® TT70 Acrylic Molding Compound
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: The ACRYLITE® Heatresist and ACRYMID® products are crystal-clear molding compounds offering higher heat deflection temperatures under load than other grades of ACRYLITE®. In fact, ACRYMID® TT70 has higher heat resistant properties than many polycarbonate grades while maintaining the excellent weatherability characteristic that is typical of acrylic.

ACRYMID® TT50 and TT70: ACRYMID® TT50 and TT70 are poly-methyl methacrylimide (PMMI) compounds that offer very high heat deflection temperatures. They are suitable for high-temperature applications such as headlamp lenses, drum lenses and built-in furniture lighting. Besides their high light transmission, clarity, excellent strength and rigidity, these specialty molding compounds offer extremely stable optical values after long-term exposure to heat.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 0.54 %0.54 %ISO 62
Water Absorption at Saturation 6.0 %6.0 %ISO 62
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inISO 294
Melt Flow 1.7 g/10 min
@Load 10.0 kg,
Temperature 260 °C
1.7 g/10 min
@Load 22.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi5 mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5 mm/min; ISO 527
Tensile Modulus 4.00 GPa580 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
CTE, linear 103 µm/m-°C
@Temperature 0.000 - 50.0 °C
57.0 µin/in-°F
@Temperature 32.0 - 122 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 149 °C300 °FISO 75
Vicat Softening Point 170 °C338 °FB/50°C; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 707
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54ISO 489
Transmission, Visible 91 %91 %ISO 13458-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik ACRYMID® TT50 Acrylic Molding Compound
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding
Lucite International Lucite® 41 Acrylic Bead Resin
Röhm Acrylite® GMS Acrylic Sheet, Aerospace Grade
Arkema Oroglas® MI-2T Acrylic

PEVONIL070 / 196274

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.