MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ExxonMobil EXACT™ 5062 Plastomer for Polymer Modification  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding and profile extrusion.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 g/cc0.0311 lb/in³ExxonMobil Method
Mooney Viscosity 27
@Temperature 125 °C
27
@Temperature 257 °F
ML (1 + 4); ASTM D1646
Melt Flow 0.50 g/10 min0.50 g/10 minExxonMobil Method
 1.1 g/10 min1.1 g/10 minExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 575715s; ASTM D2240
Tensile Strength at Break >= 4.20 MPa>= 609 psiASTM D638
Elongation at Break >= 2000 %>= 2000 %ASTM D638
Flexural Modulus, 1% Secant 5.54 MPa803 psiASTM D790
Instrumented Impact Total Energy  16.3 J
@Temperature 23.0 °C
12.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 25.8 J
@Temperature -40.0 °C
19.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
Instrumented Impact Energy at Peak  13.6 J
@Temperature 23.0 °C
10.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 14.9 J
@Temperature -40.0 °C
11.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
Tear Strength 28.0 kN/m160 pliDie C; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 42.8 °C109 °FPeak Melting Temperature; ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 6.0 %
@Thickness 1.27 mm
6.0 %
@Thickness 0.0500 in
ASTM D1003
 
Descriptive Properties
Failure ModeDUCTILE23°C and 40°C
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer
ExxonMobil EXACT™ SLP-9087 Plastomer for Extrusion Coating Applications
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin

PEXB367 / 37672

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.