MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ExxonMobil LLDPE LL 6202.19 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear resistance and low warpage.

Availability: Latin America, North America and South America

Applications:

  • Caps
  • Closures
  • Lids

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ExxonMobil method
ESCR 10% Igepal® 180 hour180 hourF50; ASTM D1693B
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 12.4 MPa1800 psiASTM D638
Elongation at Break 750 %750 %ASTM D638
Flexural Modulus 0.407 GPa
@Strain 2 %
59.0 ksi
@Strain 2 %
Secant; ASTM D638
Flexural Modulus, 1% Secant 455 MPa66000 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 123 °C<= 254 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ PL 1840 Polyolefin Plastomer
ExxonMobil LL 6202.19 Injection Molding Resin
ExxonMobil LLDPE LL 6201.19 Linear Low Density Polyethylene Resin
A. Schulman CP814-01 Linear, Low-Density Polyethylene
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene

PEX99170 / 175406

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.