MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: CoPA, injection molding grade, 30% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 130, conditioning may be unnecessary in single cases, good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183
Water Absorption 6.0 %6.0 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 1.8 %1.8 %23°C/50% R.H.; Test Sim. to ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiConditioned; ISO 527-1/-2
 130 MPa18900 psiISO 527-1/-2
Elongation at Break 3.5 %3.5 %ISO 527-1/-2
 8.0 %8.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 4.40 GPa638 ksiConditioned; ISO 527-1/-2
 8.10 GPa1170 ksiISO 527-1/-2
Charpy Impact Unnotched  9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 4.50 J/cm²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Impact 13031303Puncture maximum force (N); ISO 6603-2
 939
@Temperature -30.0 °C
939
@Temperature -22.0 °F
Puncture maximum force (N); ISO 6603-2
Puncture Energy 7.00 J5.16 ft-lbISO 6603-2
 4.00 J
@Temperature -30.0 °C
2.95 ft-lb
@Temperature -22.0 °F
ISO 6603-2
 4.00 J
@Temperature -30.0 °C
2.95 ft-lb
@Temperature -22.0 °F
Conditioned; ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 450 V450 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-1/-2
Melting Point 213 °C415 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
Vicat Softening Point 200 °C392 °F50°C/h 50N; ISO 306
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
IEC 60695-11-10
 
Descriptive Properties
FeaturesHeat stabilized or stable to heat
 High impact or high impact modified
FormPellets
ISO Short NameISO 1874-PA 6/66-HI, MHR, -080, GF30
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo PULSE™ A35-105 PC/ABS
INEOS Styrolution Terluran® GP-25 ABS
INEOS Styrolution Terluran® GP-22 ABS
Claude Bamberger Bamberko® 9016 Purge Compound

PLANX0760 / 98975

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.