MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kaneka PHBH Rigid Bio-based Polymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions), hydrolytic stability, and heat resistance.

Information provided by Kaneka Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Vapor Transmission 80.0 - 120 g/m²/day
@Thickness 0.0600 mm
5.15 - 7.73 g/100 in²/day
@Thickness 0.00236 in
film; JIS Z0208
Oxygen Transmission 0.300 - 0.900 cc-mm/m²-24hr-atm
@Thickness 0.0600 mm
0.762 - 2.29 cc-mil/100 in²-24hr-atm
@Thickness 0.00236 in
film; JIS Z7126
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 28.0 MPa4060 psi100 micron film; ASTM D882
Elongation at Break 26 %26 %100 micron film; ASTM D882
Tensile Modulus 1.24 GPa180 ksi100 micron film; ASTM D882
Flexural Modulus 1.53 GPa222 ksiASTM D790
Izod Impact, Notched 0.330 J/cm0.618 ft-lb/inASTM D256
Tear Strength 77.0 kN/m439 pli100 micron film; ASTM D1004
 
Thermal PropertiesMetricEnglishComments
Melting Point 142 °C288 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FASTM D48
Vicat Softening Point 117 °C
@Load 1.02 kg
243 °F
@Load 2.25 lb
Glass Transition Temp, Tg 2.00 °C35.6 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 40 %
@Thickness 0.100 mm
40 %
@Thickness 0.00394 in
film; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kaneka PHBH Semi-Rigid Bio-based Polymer
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend
GEHR Plastics ECOGEHR® PLA-WF Polylactic Acid, 30% Wood Fibers
Telles M-vera™ B5008 Film Grade Compostable Bioplastic
LATI Latigea B01 F1 Bio-Polymer

PKANEKA90 / 142924

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.