MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Plenco 08218 Polyester BMC, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make it suitable for a broad range of applications. Because of its excellent electrical resistance and mechanical strength, it is well suited to commercial/industrial heavy duty electrical parts, including enclosures for power distribution equipment, fuse holders, circuit breaker cases, electric motor housings and components. It is available in bulk or extruded form, and currently in the colors of natural and light gray. Other colors available upon request. It is UL recognized under file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.83 g/cc0.0661 lb/in³ASTM D792
Water Absorption 0.091 %0.091 %ASTM D570
Linear Mold Shrinkage 0.0038 cm/cm0.0038 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 4646ASTM D785
Tensile Strength, Ultimate 46.0 MPa6670 psiASTM D638
Elongation at Break 0.59 %0.59 %ASTM D638
Tensile Modulus 13.2 GPa1910 ksiASTM D638
Flexural Strength 133 MPa19300 psiASTM D790
Flexural Modulus 12.4 GPa1800 ksiASTM D790
Compressive Strength 136 MPa19700 psiASTM D695
Poissons Ratio 0.2960.296ASTM D638
Shear Modulus 5.09 GPa738 ksiCalculated
Izod Impact, Notched 4.30 J/cm8.06 ft-lb/inASTM D256
Charpy Impact, Notched 4.30 J/cm²20.5 ft-lb/in²ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.30e+15 ohm-cm2.30e+15 ohm-cmASTM D247
Dielectric Constant 4.44.4ASTM D150
Dielectric Strength 10.9 kV/mm277 kV/inStep by Step; ASTM D149
 13.5 kV/mm343 kV/inShort Time; ASTM D149
Dielectric Breakdown 22645 V22645 V1hr 120C; ASTM D149
Dissipation Factor 0.02290.0229ASTM D150
Arc Resistance 191 sec191 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 222 °C432 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 271 °C520 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.0013 %0.0013 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® IG454-A Compression Molded HDPE Resin
Mid-Mountain Materials ARMATEX® SF17 Silicone Rubber Coated Glass Fabric
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade
Prodways TPU-70 A Powder for Laser Sintering

PLEM55m3 / 50741

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.