MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chevron Phillips HiD® 9300 HDPE Orange Pipe Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Resin Type: Linear Copolymer; PE2406 Pipe Resin; ASTM D 3350 Classification: 234363E; ASTM D 4976 Classification: PE 225, A 56607

Characteristics: PPI Recommended Hydrostatic Design Bases (HDB): 1250 psi at 73°F, 1000 psi at 140°F

Applications:Natural Gas Distribution Piping and Fittings

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Environmental Stress Crack Resistance  >= 2000 hour
@Temperature 50.0 °C
>= 2000 hour
@Temperature 122 °F
F50, Cond. B.; ASTM D1693
 >= 5000 hour
@Temperature 100 °C
>= 5000 hour
@Temperature 212 °F
F50 Cond. C; ASTM D 1693
Melt Flow 0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Ultimate 31.0 MPa4500 psiASTM D638
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Stiffness Modulus 0.790 GPa115 ksi3 pt. secant ASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 120 °C248 °FASTM D1525
Brittleness Temperature <= -59.0 °C<= -74.2 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Versalis Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin

PCHEVV45 / 20441

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.