MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Sanitary gaskets made from Fluoraz® 784 work well in Sip and CIP applications where a low durometer elastomer compound is needed. While EPDMs and FKMs can provide a seal for extended periods, changes in physical properties can have adverse effects beyond simple volume swell. A decrease in hardness or drop in modulus signals a reduction in compressive strength. If a sanitary gasket is retorqued to the installations specification, the gasket will be compressed at a greater level than desired, resulting in increased intrusion into the process stream. An increase in hardness/modulus and a drop in elongation means embrittlement. The seal will be undertorqued, resulting in either leaks or cracking.

Fluoraz 784 is formulated for use in sanitary gaskets and other applications where low sealing force is required, such as sealing sight glasses or as a seal between nonmetal parts. Fluoraz 784 is FDA and USP Class VI compliant, making it a versatile compound for both pharmaceutical and other hygienic fluid handling applications. Fluoraz 784 metal and TOC extractables are an order of magnitude lower than premium competitive FKM formulations, ensuring little or no contamination into the process stream. Fluoraz 784 can be used as sanitary gaskets in standard applications as long as the toque used to install the gasket is minimal (hand tight).

Fluoraz 784 is also available in O-rings and custom shapes where a low durometer hardness is desired.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 19.82 MPa2875 psiASTM D1414
Tensile Strength, Yield 2.62 MPa380 psi@100% Elongation; ASTM D1414
Elongation at Break 342 %342 %ASTM D1414
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -6.67 °C20.0 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM
Garlock 2264 C.I. EPDM Sheet Rubber, Polyester Insert
Garlock 563 EPDM Sheet Rubber
Garlock STRESS SAVER® 370 EPDM/PTFE Gasketing
Garlock 8316 EPDM Sheet Rubber Gasketing

PGREEN39 / 42333

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.