MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Outokumpu 4313 Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: Applications: Wet corrosion resistance and general service.

Available in hot rolled plate (Quarto) form.

Key Words: EN 1.4313; UNS S41500; JIS SUS Ti6NM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 850 MPa123000 psiOutokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield  650 MPa
@Strain 0.2 %
94300 psi
@Strain 0.2 %
EN min., RT; EN 10002-1
 700 MPa
@Strain 0.2 %
102000 psi
@Strain 0.2 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
 770 MPa
@Strain 1 %
112000 psi
@Strain 1 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
 530 MPa
@Strain 0.2 %,
Temperature 400 °C
76900 psi
@Strain 0.2 %,
Temperature 752 °F
EN min.; EN 10002-5
 560 MPa
@Strain 0.2 %,
Temperature 200 °C
81200 psi
@Strain 0.2 %,
Temperature 392 °F
EN min.; EN 10002-5
 590 MPa
@Strain 0.2 %,
Temperature 100 °C
85600 psi
@Strain 0.2 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 20 %20 %Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Chromium, Cr 13 %13 %
Iron, Fe 82.45 %82.45 %
Molybdenum, Mo 0.50 %0.50 %
Nickel, Ni 4.0 %4.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness
Aluminum 7175-T7351
CA6NM Martensitic Stainless Steel, Annealed Bar, Forgings, UNS S41500
Schmolz + Bickenbach UGICHROM 4507 Duplex Chrome Plated Bar
316 Stainless Steel, annealed bar

NOUTOK03 / 18718

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.