MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers TEKAPPO® JF101 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance and reinforced fiberglass. It shows high dimensional stability and rigidity used for housing and electrical parts.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0045 cm/cm0.0045 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.917 MPa8110.1 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Strength 103.01 MPa14940 psiASTM D790
Flexural Modulus 4.199 GPa609.0 ksiASTM D790
Izod Impact, Notched 0.539 J/cm1.01 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FASTM D648
Flammability, UL94 V-1V-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 300 °C464 - 572 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 257 PPO
Kraton® G1650 + PPE blend (10/90)
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
Evonik Vestoran® 1900-GF20 nf PPE
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 100 Gauge

PEPOLZ048 / 103545

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.