MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

PTS PCA-3013 High Flow PC/PBT Alloy
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Information provided by Polymer Technology and Services, LLC (PTS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inASTM D955
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 250 °C
20 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.7 MPa
@Thickness 3.17 mm
7500 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 150 %
@Thickness 3.17 mm
150 %
@Thickness 0.125 in
ASTM D638
Flexural Yield Strength 63.4 MPa
@Thickness 3.17 mm
9200 psi
@Thickness 0.125 in
ASTM D790
Flexural Modulus 1.83 GPa
@Thickness 3.17 mm
265 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 6.94 J/cm
@Thickness 3.17 mm
13.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FASTM D648
UL RTI, Electrical 75.0 °C167 °F
UL RTI, Mechanical with Impact 75.0 °C167 °F
UL RTI, Mechanical without Impact 75.0 °C167 °F
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 238 - 249 °C460 - 480 °F
Middle Barrel Temperature 243 - 260 °C470 - 500 °F
Front Barrel Temperature 252 - 274 °C485 - 525 °F
Nozzle Temperature 252 - 263 °C485 - 505 °F
Melt Temperature 249 - 271 °C480 - 520 °F
Mold Temperature 65.6 - 82.2 °C150 - 180 °F
Drying Temperature 121 °C250 °F
Dry Time 2 - 4 hour2 - 4 hour
Back Pressure 1.72 - 3.45 MPa250 - 500 psi
Shot Size 50 - 80 %50 - 80 %
Screw Speed 25 - 50 rpm25 - 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
PTS PBT-15GF 15% Glass Filled PBT

PZ9PU44 / 21582

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.