MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Processed by selective laser sintering (SLS). Windform® SP is a deep black composite polyamide that is a “Top” level material within the polyamide Windform® materials for additive manufacturing. It has excellent mechanical properties similar to Windform XT 2.0. In addition it has the added advantage of increased resistance to shocks, vibrations and deformations. This material shows increases in impact strength and elongation at break. Moreover the Windform® SP retains its excellent thermal properties and resistance to high temperature. Windform® SP parts have high mechanical characteristics per weight.

Uses: Windform® SP is suitable to create accurate and reliable prototypes and is perfect for functional applications in motorsports, automotive (suitable for example for components under the hood, such as intake manifolds), Air (components for UAV , Unmanned Aerial Vehicle) and aerospace design, since it allows applications fully functional as well as dyno tests, track tests and development of pre-serie parts. It is also recommended for all applications requiring resistance to damage, vibration and deformation. These applications only examples; the versatility of the product combined with the technology used allows infinite possibilities. Another important element of this material is its resistance to absorption of liquids and moisture.

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.106 g/cc0.03996 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 76.10 MPa11040 psiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 11.38 %11.38 %UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 6.2196 GPa902.09 ksiUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 120.08 MPa17416 psiUNI EN ISO 14125: 2000
Flexural Modulus 4.647 GPa674.1 ksiUNI EN ISO 14125: 2000
Charpy Impact Unnotched 2.868 J/cm²13.65 ft-lb/in²UNI EN ISO 179-1
Charpy Impact, Notched 0.582 J/cm²2.77 ft-lb/in²UNI EN ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+8 ohm-cm<= 1e+8 ohm-cmASTM D257-93
Surface Resistance <= 1e+8 ohm<= 1e+8 ohmASTM D257-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 193.3 °C379.9 °FISO 11357-2
Deflection Temperature at 1.8 MPa (264 psi) 186.5 °C367.7 °FASTM D648 Type B
Vicat Softening Point 189.9 °C373.8 °F10 N; ASTM D1525-09
 
Descriptive Properties
ColorDeep Black
Specific Flexural Modulus4201.99[MPa/(g/cc)], Flexural Modulus per density unit
Specific Flexural Strength108.57[MPa/(g/cc)], Flexural Strength per density unit
Specific Tensile Modulus5623.51[MPa/(g/cc)], Tensile Modulus per density unit
Specific Tensile Strength68.81[MPa/(g/cc)], UTS per density unit
Surface Finish1.15 Ra µmAfter CNC Machining
 1.45 Ra µmAfter Manual Finishing
 6.2 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite
CRP Technology Windform® LX 2.0 Polyamide Composite
Prodways PLASTCure ABS 3650 3D Printing Polymer
Overview of materials for Nylon 12

PCRPT45 / 138472

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.