MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LNP Faradex DS-1003 FR HI EXP Polycarbonate, Stainless Steel Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Stainless Steel Fiber

Material Notes:
  • Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically Conductive, Flame Retardant, Low to None Halogen Content, ECO Compliant, High Impact Resistance
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psiISO 527-1, -2
Elongation at Break 4.0 - 8.0 %4.0 - 8.0 %ISO 527-1, -2
Flexural Strength 80.0 MPa11600 psiISO 178
Flexural Modulus 2.60 GPa377 ksiISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) 85.0 kJ/m²40.4 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D4496
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.0 µm/m-°C
@Temperature 20.0 °C
37.2 µin/in-°F
@Temperature 68.0 °F
ISO 11359-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FUnannealed; ISO 75A-1, -2
Flammability, UL94 V-0
@Thickness 2.10 mm
V-0
@Thickness 0.0827 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 304 - 327 °C579 - 621 °F
Mold Temperature 93.3 - 121 °C200 - 250 °F
Drying Temperature 121 - 149 °C250 - 300 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa24.9 - 50.0 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LNP Faradex AS-1002 Acrylonitrile Butadiene Styrene, Stainless Steel Fiber

PZLNP1031 / 51113

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.