MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Interleave: Polyethylene
Side 1: Cured Silicone Rubber
Carrier: PTFE Coated Fiberglass

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 457 microns18.0 milOverall; Arlon SQA-TMS-003
 457 microns18.0 milSide 1; Arlon SQA-TMS-003
 457 microns18.0 milInterleave
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040Silicone Property; ASTM D2240
Tensile Strength 8.62 MPa1250 psiSilicone Property; ASTM D412
Elongation at Break 800 %800 %Silicone Property; ASTM D412
Tear Strength 38.6 kN/m220 pliDie B, Silicone Property; ASTM D624
Compression Set 19 %19 %Arlon SQA-TMS-017
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 50.20 kV/mm1275 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Postcure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 60.0 Month
@Temperature 23.9 °C
60.0 Month
@Temperature 75.0 °F
From date of manufacture
 
Descriptive Properties
ColorSaddle Brown
Total Product Weight (oz/yd2)15.1Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories 1500 ACE BLANKET Blanket
Sinotek Materials Packing PTFE Braided with Graphite
Aremco Pyro-Putty™ 1500 High Temperature Ceramic-Metallic Putty, Ceramic Filled
Rogers Arlon CLTE Microwave Printed Circuit Board Substrate
Rogers Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

PARL661 / 125847

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.