MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 4605 Syndiotactic Polystyrene (SPS), Glass Fiber
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS); Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D 792
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D 570
Additive Loading 30 %30 %Primary Additive
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.20 mm
0.0030 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 121 MPa17500 psiASTM D 638
Elongation at Break 1.6 %1.6 %ASTM D 638
Tensile Modulus 9.65 GPa1400 ksiASTM D 638
Flexural Strength 169 MPa24500 psiASTM D 790
Flexural Modulus 9.65 GPa1400 ksiASTM D 790
Izod Impact, Notched 0.961 J/cm
@Thickness 3.20 mm
1.80 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 293 - 327 °C560 - 620 °F
Mold Temperature 71.1 - 149 °C160 - 300 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled
RTP Company RTP 4607 HI FR Syndiotactic Polystyrene (SPS), Glass Fiber - Impact Modified - Flame Retardant
RTP Company RTP 1302 Polyphenylene Sulfide (PPS), Glass Fiber - UL94 V-0
RTP Company RTP 4607 FR Syndiotactic Polystyrene (SPS), Glass Fiber - Flame Retardant

PQZWA8556 / 92392

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.