MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Struktol VLB 618 Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Blend of fatty acid esters. STRUKTOL® VLB-618 is manufactured from high quality vegetable fatty acids.

Applications: STRUKTOL® VLB-618 is the vegetable version of VLB-602 and is a very compatible complex ester lubricant. It has noted performance in clear calendared PVC sheet. It also has application in clear extrusion, blow molding and injection molding formulations. It is especially useful in products that require printing, laminating, or bonding. STRUKTOL® VLB-618 is very effective mostly as an external lubricant, with some internal properties, which have no negative impact on clarity in extrusion, calendering, or injection molding. STRUKTOL® VLB-618 is noted to have ideal characteristics for calendared sheet where clarity and low water blush is critical and where lower cost in performance is needed to replace montanic esters.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.025 g/cc1.025 g/cc
 
Thermal PropertiesMetricEnglishComments
Dropping Point 79.0 - 88.0 °C174 - 190 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
AppearanceOff white to tan pastille or powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALKAMIDE® C 212 Surfactant
Versalis Europrene® 1723 Emulsion Styrene-Butadiene Rubber
Trinseo BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
LG Chemical NBR 7150 High Acrylonitrile Polymer
KKPC KOSYN 1502LL Styrene Butadiene Rubber

PSTRUK50 / 69277

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.