MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling SUSTAPEEK® GF 30 PEEK, 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes:
  • High rigidity at good dimensional stability
  • Very low creep tendency
  • High continuous service temperature
Product applications:
  • Electrical industry
  • Aviation industry
  • Chemical engineering and tank building

Information provided by Röchling.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.30 %0.30 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 105105ASTM D785
Hardness, Rockwell R 126126ASTM D785
Hardness, Shore D 8686ASTM D2240
Tensile Strength, Yield 165 MPa24000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 8.96 GPa1300 ksiASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
Flexural Modulus 9.31 GPa1350 ksiASTM D790
Compressive Strength 179 MPa26000 psiASTM D695
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM D696
Thermal Conductivity 0.422 W/m-K2.93 BTU-in/hr-ft²-°F
Melting Point 341 °C645 °FASTM D789
Maximum Service Temperature, Air 266 °C510 °F
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
NSF NoNo
USDA NoNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-20GFR 20% Glass Reinforced Polycarbonate With Release
Overview of materials for Chlorinated PVC (CPVC)
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled
Röchling SUSTAPEEK® PEEK
Röchling SUSTAPEEK® PEEK

PROCH9056 / 232759

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.