MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed CHEMRAZ® 570 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent performance in long-term static photolithography, acid/solvent and ultrapure H2O applications

Applications:

  • Valve seals
  • Fitting and union seals
  • Gaskets
  • Regulator seals
  • Filter seals
  • Dispensing seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.98 g/cc1.98 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength at Break 8.96 MPa1300 psiASTM D1414
Tensile Strength, Yield 2.41 MPa350 psi@50% Elongation; ASTM D1414
 5.38 MPa780 psi@100% Elongation; ASTM D1414
Elongation at Break 145 %145 %ASTM D1414
Compression Set 35 %
@Temperature 204 °C,
Time 252000 sec
35 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 210 °C410 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer
Greene Tweed CHEMRAZ® 600 Perfluoroelastomer
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer

PGREEN17 / 42311

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.