MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long carbon fibers. Grivory GCL-3H anthracite is characterized by the following key-properties:
  • very high stiffness and strength even after conditioning and over a wide temperature range
  • excellent notched impact resistance also at low temperatures
  • low creep
  • high heat distortion temperatures
  • low moisture absorption
  • very good dimensional stability and little warpage
  • very little coefficient of thermal expansion
  • very low density
Grivory The product has been designed for injection molding of technical parts especially in the area of light weight metal and composite replacement. Grivory GCL-3H anthracite is used in the following market segments:
  • sports & leisure
  • automotive
  • mechanical engineering
The carbon fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³Dry; ISO 1183
Water Absorption 4.7 %4.7 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 285 MPa41300 psiConditioned; ISO 2039-1
 320 MPa46400 psiDry; ISO 2039-1
Tensile Strength at Break 270 MPa39200 psiConditioned; ISO 527-1/-2
 315 MPa45700 psiDry; ISO 527-1/-2
Elongation at Break 1.6 %1.6 %Dry; ISO 527-1/-2
 1.7 %1.7 %Conditioned; ISO 527-1/-2
Tensile Modulus 21.5 GPa3120 ksiConditioned; ISO 527-1/-2
 22.5 GPa3260 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 30 ohm-cm30 ohm-cmDry; IEC 60093
 30 ohm-cm30 ohm-cmConditioned; IEC 60093
Surface Resistance 50 ohm50 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C212 - 248 °FLong Term; ISO 2578
 220 °C428 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 240 °C464 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Exterior
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsConnectors
 Electrical appliances
 Electrical equipment
 Energy distribution
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Product AttributesLong Fiber Reinforced
Special CharacteristicsAnti-static
 Improved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HT XE 3996 PA*-GF30
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Arkema Rilsan® HT CZM 30 BLACK TLD PA-GF30
EMS-Grivory Grivory® GC-4H PA*-CF40

PGRH317 / 157026

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.