MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Natural Rubber, Vulcanized (NR, IR, Polyisoprene)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.

Natural rubber usually withstands polar organic solvents (alcohols, ketones, aldehydes), organic acids, and mild chemicals. Its is adversely affected by most hydrocarbons, oil/grease/fat, strong acid, and ozone.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³Uncompounded
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 10030 - 100Depends on compounding
Hardness, Shore D 30 - 4530 - 45Depends on compounding
Tensile Strength, Ultimate 28.0 MPa4060 psiCompounded Tire
Elongation at Break 100 - 800 %100 - 800 %
100% Modulus 1.50 MPa
@Strain 100 %
218 psi
@Strain 100 %
Shear Modulus 0.000500 GPa0.0725 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cm
Dielectric Constant 2.9
@Frequency 1000 Hz
2.9
@Frequency 1000 Hz
Dielectric Strength 50.0 kV/mm1270 kV/inStep by step
Dissipation Factor  0.0020
@Frequency 60.0 - 1000 Hz
0.0020
@Frequency 60.0 - 1000 Hz
 0.030
@Frequency 1e+6 Hz
0.030
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 225 µm/m-°C
@Temperature 20.0 °C
125 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.440 J/g-°C0.105 BTU/lb-°F
Thermal Conductivity 0.150 W/m-K1.04 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5261.526

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Overview of materials for Silicone Rubber
ATG s.r.l. NR Natural Rubber
Butyl Rubber (IIR, CIIR, BIIR)
Metflex EM67 Natural Rubber

P0RUB1 / 20064

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.