MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

ALM PA 850 Black Nylon 11 SLS Prototyping Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11)

Material Notes:

Information provided by Advanced Laser Materials (ALM).

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 g/cc0.0181 lb/in³ASTM D1895
Density 1.03 g/cc0.0372 lb/in³Sintered Part; ASTM D792
Particle Size 50 µm50 µmAverage D50; Laser Diffraction
 38 - 78 µm38 - 78 µmRange (D10 to D90); Laser Diffraction
Melt Flow 26 g/10 min
@Load 5.00 kg,
Temperature 235 °C
26 g/10 min
@Load 11.0 lb,
Temperature 455 °F
3 min.; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474ASTM D2240
Tensile Strength at Break 48.0 MPa6960 psiXY direction; ASTM D638
Tensile Strength, Ultimate 42.0 MPa6090 psiZ direction; ASTM D638
Elongation at Break 14 %14 %Z direction; ASTM D638
 51 %51 %XY direction; ASTM D638
Tensile Modulus 1.43 GPa207 ksiZ direction; ASTM D638
 1.48 GPa215 ksiXY direction; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.3e+13 ohm-cm1.3e+13 ohm-cm50% RH; 500V; ASTM D257
Surface Resistance 4.9e+12 ohm4.9e+12 ohm50% RH; 500V; ASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear  120 µm/m-°C
@Temperature 0.000 - 50.0 °C
66.7 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831
 342 µm/m-°C
@Temperature 85.0 - 145 °C
190 µin/in-°F
@Temperature 185 - 293 °F
ASTM E831
Melting Point 200 °C392 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
ALM PA 650 Nylon 12 SLS Prototyping Polymer
CRP Technology Windform® RL Thermoplastic Elastomer for SLS
ALM D80-ST Nylon 11 SLS Prototyping Polymer
ALM PA 860 White Nylon 11 SLS Prototyping Polymer

PALAP97 / 176027

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.