MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm CYROLITE® Protect 2 Acrylic-polycarbonate alloy  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic/Polycarbonate Alloy

Material Notes: CYROLITE® Protect and CYROLITE® Protect 2 acrylic-based multipolymer compounds and CYREX® Protect acrylic-polycarbonate alloy provide antimicrobial capabilities* against a variety of microorganisms commonly found in healthcare facilities. Antimicrobial products are used in medical devices for secondary infection management or to inhibit bacterial growth.

Benefits:

  • Antimicrobial capabilities within the polymer structure. No secondary operations required.
  • Chemical resistance to lipids and alcohol
  • Easily welded
  • Bondable to PVC tubing
  • Excellent impact strength
  • EtO, gamma and e-beam sterilizable
Transparent blue tint, free of bisphenol A (BPA), superior resistance to lipids and alcohol as well as excellent ductility

The former Cyro/Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 230 °C
10 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 47.2 MPa6850 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Tensile Modulus 2.10 GPa305 ksiASTM D638
Flexural Strength 70.2 MPa10200 psiASTM D790
Flexural Modulus 2.20 GPa319 ksiASTM D790
Izod Impact, Notched (ISO) 1.30 kJ/m²
@Thickness 6.35 mm,
Temperature 23.0 °C
0.619 ft-lb/in²
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 100 °C212 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 48 %
@Thickness 3.00 mm
48 %
@Thickness 0.118 in
ASTM D1003
Transmission, Visible 40 %
@Thickness 3.00 mm
40 %
@Thickness 0.118 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 249 °C450 - 480 °F
Mold Temperature 50.0 - 82.0 °C122 - 180 °F
Drying Temperature 79.0 °C174 °FPredrying
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourPredrying

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik CYROLITE® Protect Acrylic-polycarbonate alloy
Prodways TPU-70 A Powder for Laser Sintering
Röhm CyRex® 100 Acrylic-Polycarbonate Alloy
RTP Company RTP 1800 A TFE 15 Polycarbonate/Acrylic Alloy (PC/PMMA), PTFE Lubricated
Röhm CYROLITE Med2 Acrylic-Based Multipolymer Compound

PEVONIL074 / 196278

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.