MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for PCTA Polyester Alloy
Categories: Polymer; Thermoplastic; Polyester, TP; PCTA Polyester Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PCTA Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Average value: 1.20 g/cc Grade Count:5
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cm0.00200 - 0.00600 in/inAverage value: 0.00400 cm/cm Grade Count:5
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103 - 105103 - 105Average value: 103 Grade Count:5
Tensile Strength, Ultimate 46.0 - 53.0 MPa6670 - 7690 psiAverage value: 49.3 MPa Grade Count:5
Tensile Strength, Yield 46.0 - 47.0 MPa6670 - 6820 psiAverage value: 46.8 MPa Grade Count:5
Elongation at Break 200 - 320 %200 - 320 %Average value: 262 % Grade Count:5
Elongation at Yield 4.00 - 5.00 %4.00 - 5.00 %Average value: 4.56 % Grade Count:5
Modulus of Elasticity 1.80 GPa261 ksiAverage value: 1.80 GPa Grade Count:3
Flexural Yield Strength 64.0 - 69.0 MPa9280 - 10000 psiAverage value: 66.9 MPa Grade Count:5
Flexural Modulus 1.75 - 2.00 GPa254 - 290 ksiAverage value: 1.91 GPa Grade Count:5
Izod Impact, Notched 0.780 - 3.70 J/cm1.46 - 6.93 ft-lb/inAverage value: 1.38 J/cm Grade Count:5
 0.400 - 0.600 J/cm
@Temperature -40.0 - -40.0 °C
0.749 - 1.12 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.438 J/cm Grade Count:4
 0.374 - 0.374 J/cm
@Temperature -40.0 - -40.0 °C
0.701 - 0.701 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.438 J/cm Grade Count:1
 0.374 - 0.374 J/cm
@Thickness 3.17 - 3.17 mm
0.701 - 0.701 ft-lb/in
@Thickness 0.125 - 0.125 in
Average value: 0.438 J/cm Grade Count:1
Izod Impact, Unnotched 99.99 - 99.99 J/cm
@Temperature -40.0 - -40.0 °C
187.3 - 187.3 ft-lb/in
@Temperature -40.0 - -40.0 °F
Grade Count:2
Izod Impact, Notched (ISO) 7.80 - 29.6 kJ/m²3.71 - 14.1 ft-lb/in²Average value: 15.1 kJ/m² Grade Count:3
 4.80 - 6.30 kJ/m²
@Temperature -40.0 - -40.0 °C
2.28 - 3.00 ft-lb/in²
@Temperature -40.0 - -40.0 °F
Average value: 5.30 kJ/m² Grade Count:3
Puncture Energy 42.0 - 3760 J31.0 - 2780 ft-lbAverage value: 980 J Grade Count:3
 48.0 - 3763 J
@Temperature -40.0 - -40.0 °C
35.4 - 2775 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 979 J Grade Count:3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 - 167 °C162 - 333 °FAverage value: 88.8 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 149 °C149 - 300 °FAverage value: 77.3 °C Grade Count:5
 
Optical PropertiesMetricEnglishComments
Haze 0.300 - 3.60 %0.300 - 3.60 %Average value: 0.960 % Grade Count:5
Transmission, Visible 77.0 - 91.0 %77.0 - 91.0 %Average value: 87.8 % Grade Count:5
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 290 °C446 - 554 °FAverage value: 265 °C Grade Count:4
Mold Temperature 15.0 - 47.5 °C59.0 - 118 °FAverage value: 29.9 °C Grade Count:4
Drying Temperature 70.0 - 95.0 °C158 - 203 °FAverage value: 76.5 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PCTG Copolyester
Eastman DURASTAR DS1010 Natural PCTA Copolyester
Eastman Eastar AN004 Natural PCTA Copolyester
Eastman Eastar BR003 Natural PCTA Copolyester
A. Schulman Diamond NPP 60-1010 PCTA Polyester Alloy

O3410 / 78210

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.