MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed CHEMRAZ® 505 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C), Chemraz 505 is the elastomer of choice for more than 90 percent of the most demanding services found in the chemical process and refining industries.

Chemraz 505 is ideal for processes taking place in subzero temperatures as well as for use in multi-substance plants or in mixed media due to its broad chemical resistance.

Chemraz 505 is available for use as O-rings, gaskets and many other custom shapes. Because of its versatility, Chemraz 505 is often used as a standard compound and can be found in a variety of applications including acids, caustics, aldehydes, esters, aromatics, hot water, steam, amines, methanol, ketones, TBA and MTBE.

Applications:

  • Mechanical seals
  • Valves
  • Pump Housings
  • Sampling/metering equipment
  • Compressors
  • Reactors
  • Mixers
  • Controls/instrumentation
  • Sprayers/dispensers
  • Couplings

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.93 g/cc1.93 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575ASTM D2240
Tensile Strength at Break 12.1 MPa1750 psiASTM D1414
Tensile Strength, Yield 3.10 MPa450 psi@ 50% Elongation; ASTM D1414
 7.93 MPa1150 psi@100% Elongation; ASTM D1414
Elongation at Break 140 %140 %ASTM D1414
Compression Set 25 %
@Temperature 204 °C,
Time 252000 sec
25 %
@Temperature 400 °F,
Time 70.0 hour
At 25% deflection; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Kalrez® 1050LF FFKM Perfluoroelastomer
Arkema Kynar® 340 PVDF-CD
Arkema KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Corning Pyrex® 7740 Borosilicate Glass Sheet
3M Dyneon™ TFE 90 Peroxide Cure Perfluoroelastomer

PGREEN01 / 42295

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.