DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability over a wide range of molding conditions. Typical applications are toys and housewares. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications. Data provided by Dow Chemical. |