MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AGC LUMIFLON® FE-4400 Isocyanate Comparison Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON fluoropolymer resins were developed in 1982 as the first solvent-soluble fluoropolymers in the world. LUMIFLON polymers consist of alternating fluoroethylene and alkyl vinyl ether segments (FEVE). The fluorinated segments provide outstanding UV stability, weather resistance, and chemical resistance, while the vinyl ether segments provide solvent compatibility and cross-linking sites. LUMIFLON resins are used to make ultra-weatherable coatings for architectural, aerospace, automotive, and industrial maintenance markets. LUMIFLON FE-4400 is a water emulsion product that was developed to meet VOC and HAPS regulations on some solvents in the U. S. FE-4400 is hydroxyl functional, and can be crosslinked with water-dispersible polyisocyanates. Like other LUMIFLON resins, FE-4400 is used to produce coatings with high gloss and excellent durability. This bulletin will compare the formulation and physical properties for two component coatings made with two different isocyanates, Bayhydur® 302 and Bayhydur 3100, both manufactured by Bayer.

Product Characteristics:

  • Moderate OH functionality
  • Excellent weathering and chemical resistance
  • High minimum film forming temperature
  • Suitable for ambient cure and bake coatings
  • Used in architectural and coil coatings

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
Solids Content 50 %50 %
Particle Size 0.10 - 0.20 µm0.10 - 0.20 µm
pH 7.0 - 9.07.0 - 9.0
 
Mechanical PropertiesMetricEnglishComments
Impact  >= 0.50
@Diameter 12.7 mm
>= 0.50
@Diameter 0.500 in
[m], Intrusion 0.5 kg, Bayhydur 302; ISO 6272
 >= 0.50
@Diameter 12.7 mm
>= 0.50
@Diameter 0.500 in
[m], Extrusion 0.5 kg, Bayhydur 3100; ISO 6272
 >= 1.0
@Diameter 12.7 mm
>= 1.0
@Diameter 0.500 in
[m], Intrusion 0.5 kg, Bayhydur 302; ISO 6272
 >= 1.0
@Diameter 12.7 mm
>= 1.0
@Diameter 0.500 in
[m], Extrusion 0.5 kg, Bayhydur 3100; ISO 6272
 
Optical PropertiesMetricEnglishComments
Gloss 55 %55 %20°, Bayhydur 302; ISO 2813
 58 %58 %20°, Bayhydur 302; ISO 2813
 81 %81 %60°, Bayhydur 3100; ISO 2813
 84 %84 %60°, Bayhydur 3100; ISO 2813
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
 
Descriptive Properties
AppearanceMilky White Liquid
Hardness4HBayhydur 3100
 HBayhydur 302
Ionic CharacterAnionic
Minimum Film Forming Temperature55°C
OH Number49[mg KOH/g]-polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay A5000 FEP Fluoropolymer
Solvay AVIMID® RB Polyimide Composite
Solvay AVIMID® N Polyimide Composite
Saint-Gobain Norton® FEP Fluoropolymer Film
Evonik Rohacell® 110EC-5 Electrically Conductive Grade Polymethacrylimide (PMI) Foam

PAGCX117 / 191226

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.