MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Overview of materials for Niobium Alloy
Categories: Metal; Nonferrous Metal; Niobium Alloy; Refractory Metal

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Niobium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.47 - 10.6 g/cc0.306 - 0.383 lb/in³Average value: 9.02 g/cc Grade Count:27
 
Chemical PropertiesMetricEnglishComments
Thermal Neutron Cross Section 1.10 barns/atom1.10 barns/atomAverage value: 1.10 barns/atom Grade Count:4
Electrode Potential -1.10 V-1.10 VAverage value: -1.10 V Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 126 - 219126 - 219Average value: 186 Grade Count:7
Hardness, Knoop 175 - 243175 - 243Average value: 220 Grade Count:6
Hardness, Rockwell B 71.0 - 97.071.0 - 97.0Average value: 88.7 Grade Count:7
Hardness, Rockwell C 16.0 - 18.016.0 - 18.0Average value: 17.5 Grade Count:4
Hardness, Vickers 50.0 - 55050.0 - 550Average value: 159 Grade Count:17
Tensile Strength, Ultimate 112 - 862 MPa16200 - 125000 psiAverage value: 456 MPa Grade Count:23
Tensile Strength, Yield 75.0 - 752 MPa10900 - 109000 psiAverage value: 363 MPa Grade Count:20
Elongation at Break 4.50 - 50.0 %4.50 - 50.0 %Average value: 20.2 % Grade Count:23
Reduction of Area 32.0 - 54.0 %32.0 - 54.0 %Average value: 44.3 % Grade Count:3
Modulus of Elasticity 68.9 - 140 GPa9990 - 20300 ksiAverage value: 105 GPa Grade Count:23
Poissons Ratio 0.350 - 0.3800.350 - 0.380Average value: 0.374 Grade Count:5
Machinability 75.0 - 80.0 %75.0 - 80.0 %Average value: 78.8 % Grade Count:4
Shear Modulus 37.3 - 38.1 GPa5410 - 5530 ksiAverage value: 37.6 GPa Grade Count:5
Shear Strength 250 - 425 MPa36300 - 61600 psiAverage value: 308 MPa Grade Count:3
Charpy Impact 81.0 - 210 J59.7 - 155 ft-lbAverage value: 143 J Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000125 - 0.0000160 ohm-cm0.0000125 - 0.0000160 ohm-cmAverage value: 0.0000144 ohm-cm Grade Count:7
Magnetic Susceptibility 0.000002280.00000228Average value: 0.00000228 Grade Count:3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.88 - 12.8 µm/m-°C3.82 - 7.10 µin/in-°FAverage value: 8.08 µm/m-°C Grade Count:16
Specific Heat Capacity 0.255 - 0.340 J/g-°C0.0609 - 0.0813 BTU/lb-°FAverage value: 0.284 J/g-°C Grade Count:18
Thermal Conductivity 41.8 - 69.6 W/m-K290 - 483 BTU-in/hr-ft²-°FAverage value: 50.3 W/m-K Grade Count:20
Melting Point 955 - 2590 °C1750 - 4690 °FAverage value: 2370 °C Grade Count:24
Solidus 955 - 2400 °C1750 - 4350 °FAverage value: 1890 °C Grade Count:3
Liquidus 970 - 2590 °C1780 - 4690 °FAverage value: 2330 °C Grade Count:13
Boiling Point 4740 - 4900 °C8570 - 8850 °FAverage value: 4780 °C Grade Count:8
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.0100 - 0.120 %0.0100 - 0.120 %Average value: 0.0200 % Grade Count:12
Hafnium, Hf 0.0100 - 30.0 %0.0100 - 30.0 %Average value: 9.28 % Grade Count:9
Hydrogen, H 0.00100 - 0.00200 %0.00100 - 0.00200 %Average value: 0.00155 % Grade Count:10
Nickel, Ni 0.00500 - 50.0 %0.00500 - 50.0 %Average value: 16.7 % Grade Count:3
Niobium, Nb (Columbium, Cb) 56.0 - 100 %56.0 - 100 %Average value: 88.9 % Grade Count:28
Nitrogen, N 0.0100 - 0.0300 %0.0100 - 0.0300 %Average value: 0.0220 % Grade Count:10
Oxygen, O 0.0150 - 0.0300 %0.0150 - 0.0300 %Average value: 0.0270 % Grade Count:10
Silicon, Si 0.00500 - 0.0300 %0.00500 - 0.0300 %Average value: 0.0133 % Grade Count:3
Tantalum, Ta 0.100 - 29.0 %0.100 - 29.0 %Average value: 7.35 % Grade Count:12
Titanium, Ti 0.700 - 44.0 %0.700 - 44.0 %Average value: 9.60 % Grade Count:5
Tungsten, W 0.0300 - 17.0 %0.0300 - 17.0 %Average value: 6.51 % Grade Count:14
Zirconium, Zr 0.500 - 3.00 %0.500 - 3.00 %Average value: 0.946 % Grade Count:12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Bronze
Overview of materials for Wrought Copper
Overview of materials for Nickel Alloy
Overview of materials for Copper Alloy
Overview of materials for Molybdenum Alloy

M01062 / 81675

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.