MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Miracll H206 Thermoplastic Polyurethane Hot Melt/Solvent Adhesive
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Good solvent solubility, fast crystallization, excellent green bonding strength and final holding strength. Applications: fabric coating, fire hose adhesive, hot melt adhesive films & tapes, solvent adhesives, etc.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Viscosity 300 - 800 cP300 - 800 cP15% in MEK, 25°C; ISO 3219
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9696ASTM D2240
Elongation at Break 600 %600 %ASTM D412
Tear Strength 35.0 kN/m200 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 10.0 min0.167 hour
 
Descriptive Properties
Minimum Activation Temperature (°C)55-65
Tfb (°C)90

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Celanese Ateva® 2810A Ethylene Vinyl Acetate Copolymer
Chemical Concepts Chem-Set™ 601 Low Temperature Hot Melt Adhesive
Chemical Concepts Chem-Set™ 707 High Performance Hot Melt
Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating

PMIRAC67 / 221396

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.