MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Vandar® 2100 PBT, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Vandar 2100 is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional stability, paintability, and toughness.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Water Absorption 0.10 %
@Temperature 22.8 °C
0.10 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inASTM D955
 0.017 - 0.022 cm/cm0.017 - 0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.022 cm/cm0.017 - 0.022 in/inISO 294-4
Melt Flow 5.5 g/10 min
@Load 5.00 kg,
Temperature 250 °C
5.5 g/10 min
@Load 11.0 lb,
Temperature 482 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 109109ISO 2039-2
Tensile Strength at Break 28.0 MPa4060 psi50mm/min; ISO 527-2/1A
Tensile Strength, Yield 40.0 MPa5800 psi50mm/min; ISO 527-2/1A
 43.4 MPa6300 psiASTM D638
Tensile Stress at Strain 26.0 MPa
@Strain 50 %
3770 psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 50 %>= 50 %
 150 %150 %ASTM D638
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 1.70 GPa247 ksi50mm/min; ISO 527-2/1A
Flexural Strength 53.0 MPa7690 psiISO 178
 60.0 MPa8700 psiASTM D790
Flexural Modulus 1.65 GPa239 ksiISO 178
 1.93 GPa280 ksiASTM D790
Izod Impact, Notched 52.9 J/cm99.0 ft-lb/inASTM D256
 1.60 J/cm
@Temperature -28.9 °C
3.00 ft-lb/in
@Temperature -20.0 °F
ASTM D256
Izod Impact, Notched (ISO) 70.0 kJ/m²33.3 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eA
 1.60 J/cm²
@Temperature -30.0 °C
7.61 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm610 kV/inIEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-2
Melting Point 225 °C437 °F10°C/min; ISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FASTM D648
 110 °C230 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 48.9 °C120 °FASTM D648
 50.0 °C122 °FISO 75-1, -2
Vicat Softening Point 137 °C279 °FISO 306
Glass Transition Temp, Tg 60.0 °C140 °FISO 11357-1,-2,-3
Flammability, UL94 HBHB
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.0 - 96.0 °C149 - 205 °Fcavity
 250 - 260 °C482 - 500 °Fhot runner
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 240 - 260 °C464 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F
 260 °C500 °FISO 294
Mold Temperature 82.0 °C180 °FISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Hold Pressure 86.0 MPa12500 psiISO 294
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Crastin® ST820 BK503 PBT-HI
Celanese Nilit FRIANYL A63 HS28 Nylon 6.6 for injection molding
Celanese Vandar® 2100UV PBT, Impact Modified
Americhem Engineered Compounds ColorFast® PCT2014 PC/PBT Alloy
Celanese Vandar® 8929 Thermoplastic Polyester Alloy

PHCQ473 / 178928

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.